Kakšni so kovalni obroči ASTM B381 Titanium zlitine?
ASTM B381 Titanium alloy forging rings is an important metal processing technology. It involves heating titanium alloy to an appropriate temperature and applying external force to induce plastic deformation at high temperatures. This process not only enhances the density and mechanical properties of titanium alloy but also refines its grain structure, improving its fatigue resistance and corrosion odpor, s čimer izpolnjuje zahteve različnih zapletenih inženirskih aplikacij .
The application scope of titanium alloy forging technology is very wide, covering aerospace, automobiles, ships, chemical industry, medical devices and other fields. In the aerospace field, through titanium alloy forging, lightweight and high-strength engine blades and aircraft structural components can be manufactured, improving the performance and safety of aircraft. In the medical device field, Kovanje titanijeve zlitine lahko ustvari umetne kosti in sklepe, ki so odporni na korozijo in biokompatibilni, ki se uporabljajo pri kirurški popravili in protetični proizvodnji .
Značilnosti ASTM B381 Titanijeve zlitine za kovanje obročev
Ključne tehnologije v kovanju zlitine iz titanijeve zlitine vključujejo: izbiro materiala, prednastavitev, ogrevanje, deformacijo kovanja, toplotno obdelavo in mehansko testiranje lastnosti itd. . Medtem ko je med njimi izbira materiala vitalnega pomena . različna kompozicija zlitin in razmerja z različnimi inženirskimi zlitinami z različnimi merilnimi zlitinami lahko prenesejo titanske zlitine z različnimi merilnimi zlitinami z različnimi merilnimi zlitinami z različnimi merilnimi zlitinami z različnimi merilnimi zlitinami z različnimi merilnimi zlitinami z različnimi merilnimi zlitinami z različnimi merilnimi zlitin zahteve .
Kovanje zlitine iz titanijeve zlitine ima odlične zmogljivosti obdelave . Različne zapletene dele in komponente je mogoče pripraviti z metodami, kot so vroče kovanje ali vroče izostatično stiskanje . zlitina titanije
Kovani deli iz titanijeve zlitine imajo značilnost visoke trdnosti, lahke in korozijske odpornosti . v primerjavi z drugimi kovinskimi materiali, zlitina titanijeve zlitine ima večje razmerje med močjo in težo in togostjo in togostjo, kar lahko zdrži večjo mehansko napetost . na istem času ima nižjo gostoto.
Kemična sestavaASTM B381 Obroči za kovanje zlitin iz titanijeve zlitine
|
Razred |
Fe |
C |
N |
H |
O |
Al |
V |
Pd |
Mo |
Ni |
Ti |
|
Gr 1 |
0.20 |
0.08 |
0.03 |
0.02 |
0.18 |
/ |
/ |
/ |
/ |
/ |
Ravnotežje |
|
Gr 2 |
0.30 |
0.08 |
0.03 |
0.02 |
0.25 |
/ |
/ |
/ |
/ |
/ |
Ravnotežje |
|
Gr 3 |
0.30 |
0.08 |
0.05 |
0.02 |
0.35 |
/ |
/ |
/ |
/ |
/ |
Ravnotežje |
|
Gr 4 |
0.50 |
0.08 |
0.05 |
0.02 |
0.40 |
/ |
/ |
/ |
/ |
/ |
Ravnotežje |
|
Gr 5 |
0.40 |
0.08 |
0.05 |
0.02 |
0.20 |
5.5~6.75 |
3.5~4.5 |
/ |
/ |
/ |
Ravnotežje |
|
Gr 7 |
0.30 |
0.08 |
0.03 |
0.02 |
0.25 |
/ |
/ |
0.12~0.25 |
/ |
/ |
Ravnotežje |
|
Gr 9 |
0.25 |
0.08 |
0.03 |
0.02 |
0.15 |
2.5~3.5 |
2.0~3.0 |
/ |
/ |
/ |
Ravnotežje |
|
Gr 12 |
0.30 |
0.08 |
0.03 |
0.02 |
0.25 |
/ |
/ |
/ |
0.2~0.4 |
0.6~0.9 |
Ravnotežje |
|
Gr23 |
0.25 |
0.08 |
0.03 |
0.01 |
0.13 |
5.5~6.5 |
3.5~4.5 |
/ |
/ |
/ |
Ravnotežje |
Mehanska lastnostodASTM B381 Obroči za kovanje zlitin iz titanijeve zlitine
|
Razred |
Natezna trdnost, min |
Moč donosa, min |
Raztezanje,% |
||
|
Ksi |
MPA |
Ksi |
MPA |
||
|
Gr 1 |
35 |
240 |
20 |
138 |
24 |
|
Gr 2 |
50 |
345 |
40 |
275 |
20 |
|
Gr 3 |
65 |
450 |
55 |
380 |
18 |
|
Gr 4 |
80 |
550 |
70 |
483 |
15 |
|
Gr 5 |
130 |
895 |
120 |
828 |
10 |
|
Gr7 |
50 |
345 |
40 |
275 |
20 |
|
Gr 9 |
90 |
620 |
70 |
483 |
15 |
|
Gr 12 |
70 |
483 |
50 |
345 |
18 |
|
Gr 23 |
120 |
828 |
110 |
759 |
10 |
AplikacijaFieldsASTM B381 TITANON ALPING COVING RINGS
V vesoljski industriji se titanijevi odkupni odplači uporabljajo za izdelavo zrakoplovov in komponent motorja . zaradi njihove lahke teže in visoke trdnosti zmanjšujejo porabo goriva in izboljšajo učinkovitost letenja .
V avtomobilski industriji se odkupni titanijevi odkupni izdelavi za izdelavo visoko zmogljivih delov motorja, kar izboljšanje zmogljivosti energije in porabe goriva vozil .
Na biomedicinskem področju je biokompatibilnost titanijevih zlitin najprimernejši material za izdelavo umetnih sklepov in kostnih vsadkov .
Glavne metode kovanjaASTM B381 Obroči za kovanje zlitin iz titanijeve zlitine
Brezplačno kovanje
Primerno za preprosto obliko, odhodi z nizko natančnostjo, odvisno od ročnega delovanja, nizka hitrost uporabe materiala . močna prilagodljivost procesa, vendar strog nadzor nad deformacijo in frekvenco kladiva .
Umre/kovanje
Odprite kovanje matrice: Uporabite matrico z utripom bliskov
Zaprto kovanje: brez zasnove bliskavice, visoka hitrost uporabe materiala, boljša natančnost, vendar stroge zahteve za nadzor moči in temperature .
Ekstruzija in valjanje
Proces ekstrudiranja skozi oblikovanje ekstrudiranja luknje, primeren za odpuščanje dolgega traku/cevi, veliko gostoto materiala, vendar veliko naložbe v opremo . krmilne oblike z neprekinjeno deformacijo, visoka učinkovitost, lahko natančno prilagodi velikost lista/profila .
Seznami naših proizvodne opreme in instrumentov za testiranje/inšpekcije
- 800 ton Hitro kovanje
- 1200 mm rezkalni stroj
- 1 -tonski stroj za kladivo
- 2 ton ingot talilna peč
- Vodoravna stružnica
- Navpična stružnica
- Natezni testirni stroj
- Ultrazvočni detektor pomanjkljivosti
- Rockwell trdota tester
O naši tovarni
We Baoji Reliab Metal Material Co.,Ltd was founded in year 2015, located in the famous 'China Titanium Valley--BAOJI', under the strong R&D ability and continuously development, our mainly products have including titanium&titanium alloy bars/rods, plates, tubes, forgings, fasteners&machined parts, also zirconium and Nickel Products . Preneseli smo sistemsko potrdilo o ISO 9001-2015, ki je namenjeno zadovoljevanjem zahtev različnih strank .
Priljubljena oznake: ASTM B381 TITAN ASLY ALLY FOVING RINGS, China ASTM B381 Titanijeve zlitine Proizvajalci, dobavitelji, tovarna